Solution polymerized polyacrylonitrile was spun, stretched, stabilized and annealed at T≥1500°C. The fiber formed contains 95% carbon. Which of the following is the fiber formed?(2)
(a) Kevlar-49
(b) PAN fiber
(c) Rayon fiber
(d) Carbon fiber
(e) Graphite fiber